Displaying all 11 publications

Abstract:
Sort:
  1. Ngah WS, Fatinathan S
    J Environ Sci (China), 2010;22(3):338-46.
    PMID: 20614774
    The study examined the adsorption of Pb(II) ions from aqueous solution onto chitosan, chitosan-GLA and chitosan-alginate beads. Several important parameters influencing the adsorption of Pb(II) ions such as initial pH, adsorbent dosage and different initial concentration of Pb(II) ions were evaluated. The mechanism involved during the adsorption process was explored based on ion exchange study and using spectroscopic techniques. The adsorption capacities obtained based on non-linear Langmuir isotherm for chitosan, chitosan-GLA and chitosan-alginate beads in single metal system were 34.98, 14.24 and 60.27 mg/g, respectively. However, the adsorption capacity of Pb(II) ions were reduced in the binary metal system due to the competitive adsorption between Pb(II) and Cu(II) ions. Based on the ion exchange study, the release of Ca2+, Mg2+, K+ and Na+ ions played an important role in the adsorption of Pb(II) ions by all three adsorbents but only at lower concentrations of Pb(II) ions. Infrared spectra showed that the binding between Pb(II) ions and the adsorbents involved mostly the nitrogen and oxygen atoms. All three adsorbents showed satisfactory adsorption capacities and can be considered as an efficient adsorbent for the removal of Pb(II) ions from aqueous solutions.
    Matched MeSH terms: Glutaral/chemistry
  2. Khanahmadi S, Yusof F, Amid A, Mahmod SS, Mahat MK
    J Biotechnol, 2015 May 20;202:153-61.
    PMID: 25481099 DOI: 10.1016/j.jbiotec.2014.11.015
    Cross-linked enzyme aggregate (CLEA) is easily prepared from crude enzyme and has many advantages to the environment and it is considered as an economic method in the context of industrial biocatalysis compared to free enzyme. In this work, a highly active and stable CLEA-lipase from cocoa pod husk (CPH) which is a by-product after removal of cocoa beans, were assayed for their hydrolytic activity and characterized under the optimum condition successfully. Face centered central composite design (FCCCD) under response surface methodology (RSM) was used to get the optimal conditions of the three significant factors (concentration of ammonium sulfate, concentration of glutaraldehyde and concentration of additive) to achieve higher enzyme activity of CLEA. From 20 runs, the highest activity recorded was around 9.407U (83% recovered activity) under the condition of using 20% saturated ammonium sulfate, 60mM glutaraldehyde as cross-linker and 0.17mM bovine serum albumin as feeder. Moreover, the optimal reaction temperature and pH value in enzymatic reaction for both crude enzyme and immobilized were found to be 45°C at pH 8 and 60°C at pH 8.2, respectively. A systematic study of the stability of CLEA and crude enzyme was taken with regards to temperature (25-60°C) and pH (5-10) value and in both factors, CLEA-lipase showed more stability than free lipase. The Km value of CLEA was higher compared to free enzyme (0.55mM vs. 0.08mM). The CLEA retained more than 60% of the initial activity after six cycles of reuse compared to free enzyme. The high stability and recyclability of CLEA-lipase from CPH make it efficient for different industrial applications.
    Matched MeSH terms: Glutaral/chemistry
  3. Fan HY, Duquette D, Dumont MJ, Simpson BK
    Int J Biol Macromol, 2018 Dec;120(Pt A):263-273.
    PMID: 30130612 DOI: 10.1016/j.ijbiomac.2018.08.084
    Composite films comprised of salmon (Salmo salar) skin gelatin and zein were prepared via crosslinking with glutaraldehyde. Response surface methodology (RSM) was used to optimize film composition to maximize tensile strength (TS) and elongation at break (EAB), and to minimize water solubility (WS) of the films. The significant (P 
    Matched MeSH terms: Glutaral/chemistry*
  4. Ong CB, Annuar MSM
    Prep Biochem Biotechnol, 2018 Feb 07;48(2):181-187.
    PMID: 29341838 DOI: 10.1080/10826068.2018.1425707
    Immobilization of cross-linked tannase on pristine multiwalled carbon nanotubes (MWCNT) was successfully performed. Cross-linking of tannase molecules was made through glutaraldehyde. The immobilized tannase exhibited significantly improved pH, thermal, and recycling stability. The optimal pH for both free and immobilized tannase was observed at pH 5.0 with optimal operating temperature at 30°C. Moreover, immobilized enzyme retained greater biocatalytic activities upon 10 repeated uses compared to free enzyme in solution. Immobilization of tannase was accomplished by strong hydrophobic interaction most likely between hydrophobic amino acid moieties of the glutaraldehyde-cross-linked tannase to the MWCNT.
    Matched MeSH terms: Glutaral/chemistry*
  5. Saravanan M, Bhaskar K, Maharajan G, Pillai KS
    J Drug Target, 2011 Feb;19(2):96-103.
    PMID: 20380621 DOI: 10.3109/10611861003733979
    We have previously reported on the targeting of diclofenac sodium in joint inflammation using gelatin magnetic microspheres. To overcome complications in the administration of magnetic microspheres and achieve higher targeting efficiency, the present work focuses on the formulation of gelatin microspheres for intra-articular administration. Drug-loaded microspheres were prepared by the emulsification/cross-linking method, characterized by drug loading, size distribution, scanning electron microscopy (SEM), Fourier transform infrared (FT-IR) spectroscopy, differential scanning calorimetry (DSC), X-ray diffraction (XRD), gas chromatography, and in vitro release studies. The targeting efficiency of microspheres was studied in vivo in rabbits. The microspheres showed drug loading of 9.8, 18.3, and 26.7% w/w with an average size range of 37-46 µm, depending upon the drug-polymer ratio. They were spherical in nature and free from surface drug as evidenced by the SEM photographs. FT-IR, DSC, and XRD revealed the absence of drug-polymer interaction and amorphous nature of entrapped drug. Gas chromatography confirms the absences of residual glutaraldehyde. The formulated microspheres could prolong the drug release up to 30 days in vitro. About 81.2 and 43.7% of administered drug in the microspheres were recovered from the target joint after 1 and 7 days of postintra-articular injection, respectively, revealing good targeting efficiency.
    Matched MeSH terms: Glutaral/chemistry
  6. Wong SHM, Lim SS, Tiong TJ, Show PL, Zaid HFM, Loh HS
    Int J Mol Sci, 2020 Jul 22;21(15).
    PMID: 32708043 DOI: 10.3390/ijms21155202
    An ideal scaffold should be biocompatible, having appropriate microstructure, excellent mechanical strength yet degrades. Chitosan exhibits most of these exceptional properties, but it is always associated with sub-optimal cytocompatibility. This study aimed to incorporate graphene oxide at wt % of 0, 2, 4, and 6 into chitosan matrix via direct blending of chitosan solution and graphene oxide, freezing, and freeze drying. Cell fixation, 3-(4,5-dimethylthiazol-2-yl)-2,5-diphenyl tetrazolium bromide, alkaline phosphatase colorimetric assays were conducted to assess cell adhesion, proliferation, and early differentiation of MG63 on chitosan-graphene oxide scaffolds respectively. The presence of alkaline phosphatase, an early osteoblast differentiation marker, was further detected in chitosan-graphene oxide scaffolds using western blot. These results strongly supported that chitosan scaffolds loaded with graphene oxide at 2 wt % mediated cell adhesion, proliferation, and early differentiation due to the presence of oxygen-containing functional groups of graphene oxide. Therefore, chitosan scaffolds loaded with graphene oxide at 2 wt % showed the potential to be developed into functional bone scaffolds.
    Matched MeSH terms: Glutaral/chemistry
  7. Taguchi K, Chuang VTG, Hashimoto M, Nakayama M, Sakuragi M, Enoki Y, et al.
    Chem Pharm Bull (Tokyo), 2020;68(8):766-772.
    PMID: 32741918 DOI: 10.1248/cpb.c20-00222
    Lactoferrin (Lf) nanoparticles have been developed as a carrier of drugs and gene. Two main methods, desolvation technique and emulsification method, for preparation of protein nanoparticles have been reported so far, but most of the previous reports of Lf nanoparticles preparation are limited to emulsification method. In this study, we investigated the optimal conditions by desolvation technique for the preparation of glutaraldehyde-crosslinked bovine Lf (bLf) nanoparticles within the size range of 100-200 nm, and evaluated their properties as a carrier for oral and intravenous drug delivery. The experimental results of dynamic light scattering and Transmission Electron Microscope suggested that glutaraldehyde-crosslinked bLf nanoparticles with 150 nm in size could be produced by addition of 2-propanol as the desolvating solvent into the bLf solution adjusted to pH 6, followed by crosslinking with glutaraldehyde. These cross-linked bLf nanoparticles were found to be compatible to blood components and resistant against rapid degradation by pepsin. Thus, cross-linked bLf nanoparticles prepared by desolvation technique can be applied as a drug carrier for intravenous administration and oral delivery.
    Matched MeSH terms: Glutaral/chemistry
  8. Jawad AH, Mubarak NSA, Abdulhameed AS
    Int J Biol Macromol, 2020 Jan 01;142:732-741.
    PMID: 31760013 DOI: 10.1016/j.ijbiomac.2019.10.014
    In this study, tunable Schiff's base-cross-linked chitosan-glutaraldehyde (CS-GLA) was modified and applied to remove reactive red 120 (RR120) dye from an aqueous solution. Different ratios of TiO2 nanoparticles, such as 25% TiO2 nanoparticles (CS-GLA/TNC-25) and 50% TiO2 nanoparticles (CS-GLA/TNC-50), were loaded into the CS-GLA's molecular structure. The adsorptive properties of CS-GLA, CS-GLA/TNC-25, and CS-GLA/TNC-50 for the RR120 dye in the aqueous solution were evaluated. CS-GLA/TNC-25 exhibited the best adsorptive property possibly because of the perfect balancing between the surface area and available amine (NH2) groups in the composite formulation. The impact of adsorption key parameters, such as adsorbent dosage (0.01-1.2 g), RR120 dye concentration (30-400 mg/L), solution pH (3-12), and contact time (0-400 min) were explored by batch adsorption mode. The adsorption was well described by the Freundlich model and pseudo-second order kinetic model. The adsorption capacity of CS-GLA/TNC-25 for RR120 dye was 103.1 mg/g at 303K. The adsorption mechanism of RR120 on the CS-GLA/TNC-25 surface can be assigned to various interactions, such as electrostatic attraction, n-π stacking, and H-bonding. Results indicate the potential application of CS-GLA/TNC-25 as environment-friendly biosorbent for removing acid and/or textile dyes, such as RR120, from aqueous environments.
    Matched MeSH terms: Glutaral/chemistry*
  9. Azman AR, Mahat NA, Abdul Wahab R, Abdul Razak FI, Hamzah HH
    Int J Mol Sci, 2018 May 25;19(6).
    PMID: 29799469 DOI: 10.3390/ijms19061576
    Waterways are popular locations for the disposition of criminal evidence because the recovery of latent fingerprints from such evidence is difficult. Currently, small particle reagent is a method often used to visualize latent fingerprints containing carcinogenic and hazardous compounds. This study proposes an eco-friendly, safranin-tinted Candida rugosa lipase (triacylglycerol ester hydrolysis EC 3.1.1.3) with functionalized carbon nanotubes (CRL-MWCNTS/GA/SAF) as an alternative reagent to the small particle reagent. The CRL-MWCNTS/GA/SAF reagent was compared with the small particle reagent to visualize groomed, full fingerprints deposited on stainless steel knives which were immersed in a natural outdoor pond for 30 days. The quality of visualized fingerprints using the new reagent was similar (modified-Centre for Applied Science and Technology grade: 4; p > 0.05) to small particle reagent, even after 15 days of immersion. Despite the slight decrease in quality of visualized fingerprints using the CRL-MWCNTS/GA/SAF on the last three immersion periods, the fingerprints remained forensically identifiable (modified-Centre for Applied Science and Technology grade: 3). The possible chemical interactions that enabled successful visualization is also discussed. Thus, this novel reagent may provide a relatively greener alternative for the visualization of latent fingerprints on immersed non-porous objects.
    Matched MeSH terms: Glutaral/chemistry
  10. Qasim SSB, Nogueria LP, Fawzy AS, Daood U
    AAPS PharmSciTech, 2020 Jun 16;21(5):173.
    PMID: 32548717 DOI: 10.1208/s12249-020-01708-x
    Innovative strategies for periodontal regeneration have been the focus of research clusters across the globe for decades. In order to overcome the drawbacks of currently available options, investigators have suggested a novel concept of functionally graded membrane (FGM) templates with different structural and morphological gradients. Chitosan (CH) has been used in the past for similar purpose. However, the composite formulation of composite and tetracycline when cross-linked with glutaraldehyde have received little attention. Therefore, the purpose of the study was to investigate the drug loading and release characteristics of novel freeze gelated chitosan templates at different percentages of glutaraldehyde. These were cross-linked with 0.1 and 1% glutaraldehyde and loaded with doxycycline hyclate. The electron micrographs depicted porous morphology of neat templates. After cross-linking, these templates showed compressed ultrastructures. Computerized tomography analysis showed that the templates had 88 to 92% porosity with average pore diameter decreased from 78 to 44.9 μm with increasing concentration. Fourier transform infrared spectroscopy showed alterations in the glycosidic segment of chitosan fingerprint region which after drug loading showed a dominant doxycycline spectral composite profile. Interestingly, swelling profile was not affected by cross-linking either at 0.1 and 1% glutaraldehyde and template showed a swelling ratio of 80%, which gained equilibrium after 15 min. The drug release pattern also showed a 40 μg/mL of release after 24 h. These doxycycline-loaded templates show their tendency to be used in a functionally graded membrane facing the defect site.
    Matched MeSH terms: Glutaral/chemistry
  11. Awang MA, Firdaus MA, Busra MB, Chowdhury SR, Fadilah NR, Wan Hamirul WK, et al.
    Biomed Mater Eng, 2014;24(4):1715-24.
    PMID: 24948455 DOI: 10.3233/BME-140983
    Earlier studies in our laboratory demonstrated that collagen extracted from ovine tendon is biocompatible towards human dermal fibroblast. To be able to use this collagen as a scaffold in skin tissue engineering, a mechanically stronger scaffold is required that can withstand manipulation before transplantation. This study was conducted to improve the mechanical strength of this collagen sponge using chemical crosslinkers, and evaluate their effect on physical, chemical and biocompatible properties. Collagen sponge was crosslinked with 1-ethyl-3-(3-dimethylaminopropyl) carbodiimide (EDC) and glutaraldehyde (GA). Tensile test, FTIR study and mercury porosimetry were used to evaluate mechanical properties, chemical property and porosity, respectively. MTT assay was performed to evaluate the cytotoxic effect of crosslinked collagen sponge on human dermal fibroblasts. The FTIR study confirmed the successful crosslinking of collagen sponge. Crosslinking with EDC and GA significantly increased the mechanical strength of collagen sponge, with GA being more superior. Crosslinking of collagen sponge significantly reduced the porosity and the effect was predominant in GA-crosslinked collagen sponge. The GA-crosslinked collagen showed significantly lower, 60% cell viability towards human dermal fibroblasts compared to that of EDC-crosslinked collagen, 80% and non-crosslinked collagen, 100%. Although the mechanical strength was better when using GA but the more toxic effect on dermal fibroblast makes EDC a more suitable crosslinker for future skin tissue engineering.
    Matched MeSH terms: Glutaral/chemistry
Filters
Contact Us

Please provide feedback to Administrator ([email protected])