OBJECTIVES: The aim of this study was to compare the biaxial flexural strength of three core ceramic materials.
MATERIAL AND METHODS: Three groups of 10 disc-shaped specimens (16 mm diameter x 1.2 mm thickness - in accordance with ISO-6872, 1995) were made from the following ceramic materials: Turkom-Cera Fused Alumina [(Turkom-Ceramic (M) Sdn Bhd, Puchong, Selangor, Malaysia)], In-Ceram (Vita Zahnfabrik, Bad Säckingen, Baden-Württemberg, Germany) and Vitadur-N (Vita Zahnfabrik, Bad Säckingen, Baden-Württemberg, Germany), which were sintered according to the manufacturer's recommendations. The specimens were subjected to biaxial flexural strength test in an universal testing machine at a crosshead speed of 0.5 mm/min. The definitive fracture load was recorded for each specimen and the biaxial flexural strength was calculated from an equation in accordance with ISO-6872.
RESULTS: The mean biaxial flexural strength values were: Turkom-Cera: 506.8 ± 87.01 MPa, In-Ceram: 347.4 ± 28.83 MPa and Vitadur-N: 128.7 ± 12.72 MPa. The results were analyzed by the Levene's test and Dunnett's T3 post-hoc test (SPSS software V11.5.0 for Windows, SPSS, Chicago, IL, USA ) at a preset significance level of 5% because of unequal group variances (P<0.001). There was statistically significant difference between the three core ceramics (P<0.05). Turkom-Cera showed the highest biaxial flexural strength, followed by In-Ceram and Vitadur-N.
CONCLUSIONS: Turkom-Cera core had significantly higher flexural strength than In-Ceram and Vitadur-N ceramic core materials.
MATERIAL AND METHOD: Two hundred discs of PEEK were prepared of 6 mm × 2 mm × 10 mm dimension. The discs were randomly divided into five groups (n = 40) for treatment, Group I: treatment with deionized distilled water (control group); Group II: PD therapy using curcumin PS; Group III: discs treated and abraded with air-borne particles (ABP) silica (30 μm particle size) modified alumina (Al); Group IV: ABP of alumina (110 μm particle size); and Group V: The PEEK were finished with 600-μm grit size straight diamond cutting bur installed in high speed hand-piece. The surface profilometer was used to evaluate the values of surface roughness (SRa) of pretreated PEEK discs. The discs were luted and bonded to discs of composite resin. The bonded PEEK samples were placed in Universal testing machine to evaluate shear BS. The type of BS failure for PEEK discs pre-treated with five regimes respectively was evaluated under stereo-microscope. The data was statistically analyzed using one-way ANOVA and the comparisons between mean values of shear BS were evaluated by Tukey's test (ρ≤0.05).
RESULTS: The PEEK samples pre-treated with diamond cutting straight fissure burs displayed statistically significant highest value of SRa values (3.258± 0.785 µm). Similarly, the shear BS was observed to be higher for the PEEK discs pre-treated with straight fissure bur (22.37±0.78 MPa). A comparable difference but not statistically significant difference was observed between PEEK discs pre-treated by curcumin PS and ABP-silica modified alumina (ρ ≥ 0.05).
CONCLUSION: PEEK discs pre-treated with diamond grit straight fissure bur displayed highest values of SRa and shear BS. It was trailed by ABP-Al pre-treated discs; whereas the SRa and shear BS values for the discs pre-treated with ABP-silica modified Al and curcumin PS did not show competitive difference.
MATERIALS AND METHODS: Forty Turkom-Cera ceramic disks (10 mm × 3 mm) were prepared and randomly divided into four groups. The disks were wet ground to 1000-grit and subjected to four surface treatments: (1) No treatment (Control), (2) sandblasting, (3) silane application, and (4) sandblasting + silane. The four groups of 10 specimens each were bonded with Panavia-F resin cement according to manufacturer's recommendations. The SBS was determined using the universal testing machine (Instron) at 0.5 mm/min crosshead speed. Failure modes were recorded and a qualitative micromorphologic examination of different surface treatments was performed. The data were analyzed using the one-way analysis of variance (ANOVA) and Tukey honestly significant difference (HSD) tests.
RESULTS: The SBS of the control, sandblasting, silane, and sandblasting + silane groups were: 10.8 ± 1.5, 16.4 ± 3.4, 16.2 ± 2.5, and 19.1 ± 2.4 MPa respectively. According to the Tukey HSD test, only the mean SBS of the control group was significantly different from the other three groups. There was no significant difference between sandblasting, silane, and sandblasting + silane groups.
CONCLUSION: In this study, the three surface treatments used improved the bond strength of resin cement to Turkom-Cera disks.
CLINICAL SIGNIFICANCE: The surface treatments used in this study appeared to be suitable methods for the cementation of glass infiltrated all-ceramic restorations.