Displaying all 4 publications

Abstract:
Sort:
  1. Arunachalam R, Rajeev V, Kumaresan R, Kurra SB
    J Contemp Dent Pract, 2019 Aug 01;20(8):952-956.
    PMID: 31797853
    INTRODUCTION: Assessment of host response to inflammation will throw light on the critical role of antioxidants (AOs) and free radicle damage in the etiology of periodontal disease. The purpose of the study was to assess the level of plasma oxidative stress in those having aggressive periodontal disease before and after full-mouth disinfection. Objectives were to find the influence of full-mouth disinfection analyzing the level of thiobarbituric acid reactive substances (TBARSs), thereby quantifying the lipid peroxidation (LPO) and also the activities of reduced glutathione (GSH), glutathione peroxidase (GPX), and catalase (CAT), valuing the AO defense systems in health and disease.

    MATERIALS AND METHODS: The valuation composed of 30 subjects with aggressive periodontal disease and 30 healthy controls. Clinical assessment included following periodontal parameters: plaque index (PI), papillary bleeding index (PBI), probing pocket depth (PPD), and clinical attachment level (CAL). Levels of bone loss were assessed by taking full-mouth periapical radiographs. Initial periodontal therapy comprises of full-mouth disinfection which includes subgingival scaling and root planing within 24 hours combined with adjunctive chlorhexidine chemotherapy for aggressive periodontitis subject's at sites indicated. The parameters (clinical) were evaluated at the baseline and 8 weeks after initial periodontal therapy at six sites of teeth indicated. Plasma samples were taken and evaluated by standard procedures as defined in the literature. All the values were weighed and related.

    RESULTS: Strong positive associations were detected among periodontal parameters and TBARS, enzymatic/nonenzymatic AO levels (p < 0.05), and pre- and postperiodontal management. The plasma levels of patients with aggressive periodontitis had high levels of TBARS and displayed a substantial escalation in the activities of GSH and GPX levels in the plasma matched to the healthy individuals (p < 0.05).

    CONCLUSION: This paper evaluated ROS activity and AO defense before and after treatment to stimulate added periodontal investigation in this part which will give an insight into the therapeutic options with foreseeable results.

  2. Alkahtani ZM, Arunachalam R, Bapat RA, Thangavelu A, Jegatheeswaran AG
    J Pharm Bioallied Sci, 2021 Jun;13(Suppl 1):S865-S867.
    PMID: 34447217 DOI: 10.4103/jpbs.JPBS_622_20
    Desquamative gingivitis is described as an erythematous, desquamated gingival lesion. There are many etiologic factors for the appearance of such lesions. The aim of this case report is to diagnose the cause of the lesion by analyzing the complete medical, dental, and personal histories. An elaborated differential diagnosis is done, and the lesion is successfully treated accordingly. The gold standard treatment is usually provided by systemic or topical corticosteroids. Another treatment option is antioxidant therapy which provides rapid healing of the tissue.
  3. Rajeev V, Arunachalam R, Nayar S, Arunima PR, Ganapathy S, Vedam V
    Eur J Dent, 2017 4 25;11(1):58-63.
    PMID: 28435367 DOI: 10.4103/ejd.ejd_113_16
    OBJECTIVE: This in vitro study was designed to assess shear bond strength (SBS) of ormocer flowable (OF) resin as a luting agent, ormocer as an indirect veneer material with portrayal of modes of failures using scanning electron microscope (SEM).

    MATERIALS AND METHODS: Sixty maxillary central incisors were divided into Group I, II, and III with 20 samples each based on luting cement used. They were OF, self-adhesive (SA) cement, and total etch (TE) cement. These groups were subdivided into "a" and "b" of ten each based on the type of veneering materials used. Veneer discs were fabricated using Ormocer restorative (O) and pressable ceramic (C). Specimens were thermocycled and loaded under universal testing machine for SBS. The statistical analysis was done using one-way ANOVA post hoc Tukey honest significant difference method.

    RESULTS: A significant difference was observed between the Groups I and II (P < 0.05). The highest mean bond strength when using ormocer veneer was obtained with the Group Ia (19.11 ± 1.92 Mpa) and lowest by Group IIa (8.1 ± 1.04 Mpa), whereas the highest mean bond strength while using ceramic veneer was of similar range for Group Ib (18.04 ± 4.08 Mpa) and Group IIIb (18.07 ± 1.40 Mpa). SEM analysis revealed OF and TE presented mixed type of failure when compared with SA where failure mode was totally adhesive.

    CONCLUSION: OF was found equally efficient like TE. Bond strength of ormocer as a veneer was not inferior to ceramic making it one of the promising additions in the field of dentistry.

Related Terms