  1. Haris NIN, Sobri S, Yusof YA, Kassim NK
    Materials (Basel), 2021 Sep 28;14(19).
    PMID: 34640054 DOI: 10.3390/ma14195657
    This study aims to develop a controlled release oil palm empty fruit bunch hemicellulose (EFB-H) inhibitor tablet for mild steel in 1 M HCl. As plant extracts tend to deteriorate at longer immersion time, limiting its industrial applicability, we attempted to lengthen the inhibition time by forming a controlled release inhibitor tablet. Electrochemical methods (potentiodynamic polarization (PDP) and electrochemical impedance spectroscopy (EIS)) were employed to investigate the efficiency and mechanism of the inhibition. An optimum dosage and immersion time was determined via Response Surface Methodology (RSM). EFB-H tablet was formulated using D-optimal mixture design, and its anticorrosion action at extended immersion time was compared with EFB-H powder. PDP measurement revealed that EFB-H is a mixed type inhibitor. RSM optimization unveiled that the optimum point for a maximum inhibition efficiency (87.11%) was at 0.33 g of EFB-H and 120 h of immersion time. Tablet T3 with EFB-H to gum Arabic to hydroxypropyl methylcellulose ratio of 66:0:34 portrayed the best tensile strength (0.243 MPa), disintegration time (152 min) and dissolution behavior. EFB-H tablet exhibited a longer-lasting inhibition effect than powder, which was 360 h as compared to 120 h for powder. Overall, EFB-H tablet has been successfully developed, and its enhanced effective inhibition time has been experimentally proven.
  2. Haris NIN, Ilyas RA, Hassan MZ, Sapuan SM, Afdzaluddin A, Jamaludin KR, et al.
    Polymers (Basel), 2021 Sep 29;13(19).
    PMID: 34641159 DOI: 10.3390/polym13193343
    This study investigates the mechanical, thermal, and chemical properties of basalt/woven glass fiber reinforced polymer (BGRP) hybrid polyester composites. The Fourier transform infrared spectroscopy (FTIR) was used to explore the chemical aspect, whereas the dynamic mechanical analysis (DMA) and thermomechanical analysis (TMA) were performed to determine the mechanical and thermal properties. The dynamic mechanical properties were evaluated in terms of the storage modulus, loss modulus, and damping factor. The FTIR results showed that incorporating single and hybrid fibers in the matrix did not change the chemical properties. The DMA findings revealed that the B7.5/G22.5 composite with 7.5 wt% of basalt fiber (B) and 22.5 wt% of glass fiber (G) exhibited the highest elastic and viscous properties, as it exhibited the higher storage modulus (8.04 × 109 MPa) and loss modulus (1.32 × 109 MPa) compared to the other samples. All the reinforced composites had better damping behavior than the neat matrix, but no further enhancement was obtained upon hybridization. The analysis also revealed that the B22.5/G7.5 composite with 22.5 wt% of basalt fiber and 7.5 wt% of glass fiber had the highest Tg at 70.80 °C, and increased by 15 °C compared to the neat matrix. TMA data suggested that the reinforced composites had relatively low dimensional stabilities than the neat matrix, particularly between 50 to 80 °C. Overall, the hybridization of basalt and glass fibers in unsaturated polyester formed composites with higher mechanical and thermal properties than single reinforced composites.
Related Terms
Filters
Contact Us

Please provide feedback to Administrator ([email protected])

External Links